ASTM A582-A582M

Home / Specifications / ASTM A582-A582M

ASTM A582 / A582M

This specification covers hot-finished or cold-finished bars, except bars for forging (Note 1), suitable for machining processes. It includes rounds, squares, and hexagons in the more commonly used types of stainless free-machining steels designed especially for optimum machinability and for general corrosion and high-temperature service. Stainless steel bars other than the free-machining types are covered in a separate specification.

astm-a582-type-347-uns-s30300-bars

ASTM A582 / A582M Chemical Requirements

UNS Designation TypeB CarbonC ManganeseC PhosphorusC SulfurC Silicon, max Chromium Nickel
S30300 303 0.15 2.00 0.20 0.15 min 1.00 17.0–19.0 8.0–10.0

BUnless otherwise indicated, a grade designation originally assigned by the American Iron and Steel Institute (AISI).
CMaximum unless otherwise noted.

ASTM A582 / A582M Mechanical Properties

Types Condition Brinell
Hardness A (HBW)
All (except 440F, 440FSe and S18235) A 262 max

ASizes below approximately 1 in. [25 mm] cross section may be tensile tested and converted to hardness per Test Methods and Definitions A370.

ASTM A582 / A582M Condition Identification

Type Condition A
(Annealed)
Condition T
(Intermediate
Temper)
Condition H
(Hard Temper)
303 A . . . . . .