ASTM A473

Home / Specifications / ASTM A473

ASTM A473

This specification covers austenitic, austenitic-ferritic,ferritic, and martensitic stainless steel forgings for general use, and for low- or high-temperature service.The values stated in inch-pound units are to be regarded as standard. The values given in parentheses are mathematical conversions to SI units that are provided for information only and are not considered standard.

astm-a473-type-347-uns-s30300-forged-bars

ASTM A473 Chemical Requirements

UNS Designation Type
Number
Carbon,
%
Manganese,
%
Phosphorus,
%
Sulfur,
%
Silicon,
%
Chromium,
%
Nickel,
%
Molybdenum,
%
S30300 303 0.15 2.00 0.20 0.15 min 1.00 17.0–19.0 8.0–10.0 0.60C

CAt manufacturer’s option; reported only when intentionally added.

ASTM A473 Mechanical Properties

Type Condition Yield Strength, min, ksi (MPa)A Tensile Strength, min, ksi (MPa) Elongation in 2 in. (50 mm) or 4D, min % Reduction of Area, min, % Brinell Hardness Number,max
303, 303SE
A 30 (205) 75 (515) 40 50 . . .

AYield strength shall be determined by the 0.2 % offset method in accordance with Test Methods and Definitions A370. An alternative method of determining yield strength may be used based on a total extension under load of 0.5 %.